Material No.: 1.4439

EN symbol (short)X2CrNiMoN17-13-5
AlloyAlloy 317 LN
UNSS 31726
Grade TP 317 LN
AFNORX2CrNiMoN17-13-5 / NF E.N 10088-1(06-2005) (FR)
BSX2CrNiMoN17-13-5 / B.S. E.N 10088-1(06-2005) (GB)

Hauptanwendungsgebiete

Chemical Industryfor processing phosphoric acid
petrochemical industry
offshore plantsSea water desalination plant
cellulose/paper industrydifferent components

Beschreibung

Densitykg/dm38,1
HardnessHB (<=35mm)
Rockwell Hardness Number max.
<=350
B90 (S 31726-ASTM A 249)
Compositionchromium nickel molybdenium steels
CategoryCorrosion resisting steels and alloys
Structureaustenitic
Corrosionresistant to intercrystalline corrosion < 400°C
non-corroding
Additional characteristicschemically resistant

Temperaturhinweise

Application area
Operation temperature-454 ºF  to 752 ºF 
temperature limit
Explanation report-454°F only in strain situation III

Chemische Zusammensetzung

Min % Max %
C0.03
Si1,00
Mn2,00
P0,045
S0,015
Cr16,5018,50
Mo4,005,00
Ni12,5014,50
Cu
N0,120,22